Ice maker injection mold | |
Mold Size |
650x550mm / advice choose 250Ton injection machine |
Mold cavity |
2+2 cavities |
Mold Steel |
718H steel, the original hardness is HRC30 degree |
Mold steel treatment way |
At final arranged thur. nitrogen for core and cavity to HRC48-52 degree surface 0.3mm thickness |
Mold gate way |
Semi hot runner system |
Mold uselife |
500000 shots |
Mold cycle time |
35 sec |
1st. Test mold time |
50 days after confirmed mold drawing files |
Mold doff way |
Choose ejectors |
Package |
PET film covered then packing into standard wooden case |
FAQ:
-How to make sure this family mould fill material even?
We arrange mold flow at beginning, then choose correct diameter for the runner & hot runner block designed different.
-How about this ice maker mold work?
It can be worked full automatic on 250Ton machine.
-For this ice maker mold if can choose more or less cavity number?
Yes, always depend on client’s demand then we will make analyse for ice maker mold.
Process | |
Mold steel |
P20, 718, 2738, 2344, 2316, S136, 3Cr13, 38CrMoAl, Mov and more |
Mold cavity |
1 or more (depend on client) |
Surface treatments |
electroplate (in order to prevent rust), thur. nitrogen (in order to rise surface hardness), vacuum quenching (in order to rise whole hardness) |
Plastic materials |
PP, PVC, PPR, ABS, PA, PC, POM, PS, PET, HDPE, LDPE and other |
Software |
UG, PRO-E, MOLDFLOW, CAD, CAE, VISI |
Mold gate way |
cold runner/hot runner/semi-hot runner |
Mold base |
HASCO, DME, LKM, HOME-MADE |
Mold doff system |
ejectors, off-plate, air valves, hydraulic jars, air jars, air ejectors, oil-motor and more |
Mold cooling |
Water cooling/air cooling/beryllium bronze cooling |
Mold payment |
50% down payment by T/T, 50% balance by T/T before shipment |
Mold shipment |
By sea/air/train |
Mold packaging |
packed into standard wooden cases |
Mold quotation |
most reasonable as rich experience |
Technology
1) Mould structure design
Professional designers provide you with reasonably designed mould to shorten cycle hours.
Reducing unnecessary procedure improves efficiency.
2) Mould cooling system
According to the structural characteristics of the product and the appearance of the product , We design a reasonable form of gate for mould, such as a large gate, hidden gate, fan gate, needle gate, pin point gate etc., a reasonable channel of runner design make mold temperature balance in the shortest time to improve mould precision and productivity.
3) Accessory for mould
Slide, guide pin, guide sleeve, lifter blocks and so on are taken by wear-resistant standard parts, to ensure the mould life.
4) Deal with mould
Quenching the mold, heat treatment to improve the hardness, then Nitriding temperature is lower , the mold will no longer need to quench mold with high surface hardness and wear resistance more than HV850
Service
1) We can repair the mould in one year for some free and provide technology. .
2) Gurantee period is 12months starting from the date of moulds accept in the Buyer’s factory.
3) If the moulds happen the big problem, The moulds cannot repaired, the Buyer cannot solve the problems,eg, mould crack, product can’t moulding…any big problem(except the human error) due to the mould life can’t reach to guranteed shots.the Seller and Buyer's negotiate to slove the problem, the buyer can send it back to the factory to repair or If serious, the Seller have resposiblity to make new mould for the Buyer.